Lightly burned magnesium is made of magnesite, which is calcined by reflective kiln, suspension kiln or boiling kiln. The product is calcined evenly, with stable quality, high purity and good activity. It is the raw material for the production of electrofused magnesium.
Technical parameters | |||||||
---|---|---|---|---|---|---|---|
Brand | MgO(%)≥ | SiO2(%)≤ | CaO(%)≤ | IgL(%)≤ | Fe2O3(%)≤ | Al2O3(%)≤ | Size(mm) |
DSM-96 | 96 | 0.45 | 1.0 | 2.0 | 0.61 | 0.16 | All kinds of particle size |
DSM-95 | 95 | 0.6 | 1.3 | 3.0 | 0.61 | 0.16 | |
DSM-94 | 94 | 1.0 | 1.4 | 4.0 | 0.61 | 0.16 | |
DSM-92 | 92 | 3.0 | 2.0 | 5.0 | 0.61 | 0.16 | |
DSM-90 | 90 | 4.0 | A grade 2.0 | 6.0 | 0.61 | 0.16 | |
B grade 2.5 | 0.61 | 0.16 | |||||
DSM-87 | 87 | 0.2 | A grade 2.0 | 7.0 | 0.61 | 0.16 | |
B grade 3.5 | 0.61 | 0.16 | |||||
DSM-85 | 85 | 6.0 | A grade 2.0 | 8.0 | 0.61 | 0.16 | |
B grade 4.0 | 0.61 | 0.16 |